dc.contributor.authorEwe, L.S.
dc.contributor.authorHamid, N.A.
dc.contributor.authorAbd-Shukor, R.
dc.date.accessioned2018-02-28T23:58:33Z-
dc.date.available2018-02-28T23:58:33Z-
dc.date.issued2006
dc.identifier.urihttp://dspace.uniten.edu.my/jspui/handle/123456789/9423-
dc.description.abstractThe insulator-metal transition temperature, Tim of Lal-x SrxMnO3 (x = 0.0, 0-05, 0.15 and 0.3) was studied during warming and cooling between 50 K to 300 K. The results showed that Tim of Lal-x SrxMnO3 shifted to a higher temperature as Sr was substituted for La. Scanning electron micrographs showed that the average grain size is in the range of 0.6 μm - 1.4 μm. Grain boundaries are almost completely revealed for x = 0.3. X-Ray powder diffraction patterns showed cubic structure (space group Pm-3m) and contain no secondary phases.
dc.titleElectrical properties and microstructure of magnetoresistive (La1-xSrxMnO3(x = 0.0, 0.05, 0.15 and 0.3)
item.fulltextNo Fulltext-
item.grantfulltextnone-
Appears in Collections:COE Scholarly Publication
Show simple item record

Google ScholarTM

Check


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.