Title: | Sinterability and mechanical properties of MnO2-doped Y-TZP: The effects of holding time variations | Authors: | Amiriyan, M. Satgunam, M. Sivakumar, S. Singh, R. Tolouei, R. |
Issue Date: | 2012 | Abstract: | the effect of holding time variation and sintering temperature on the mechanical properties and sinterability of yttria stabilized tetragonal zirconia doped with 1 wt. % MnO 2 was investigated. Samples were sintered at 1150-1500 °C with holding times varying from 12 and 120 minutes. Comparing to the MnO 2-doped Y-TZP, longer holding time resulted in enhanced densification of the undoped Y-TZP samples. In the case of MnO 2-doped Y-TZP however, Bulk density, Young's modulus, Vickers hardness and fracture toughness results show the beneficial effect of MnO 2 in enhancing the densification of Y-TZP ceramics. © (2012) Trans Tech Publications, Switzerland. | URI: | http://dspace.uniten.edu.my/jspui/handle/123456789/7581 |
Appears in Collections: | COE Scholarly Publication |
Show full item record
Google ScholarTM
Check
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.